Paint Pail Mould Suppliers introduced that plastic product bursting is a quality problem that often occurs in injection molded parts processing manufacturers. This nature is very serious. It is mainly caused by how the black material bursts. Customers generally doubt whether it is the nozzle material. too much. Because the filler material is a cause of bursting.
There is also a kind of burst with just a light press. The position is mainly the bonding line, that is, when the injection point is designed by the injection molding manufacturer, the welding line is not designed in place, and the welding line is made on the top with the bump. It also depends on the thinner position outside. Especially in the production of ABS materials, it is easy to break. An experienced design engineer will first review the glue inlet point, and then drive the weld line to a position where it will not burst.
After the injection molding employees of the injection molding parts processing factory left their jobs for more than 20 minutes, when they returned to the job, they did not shoot out the waste rubber that had been in the barrel for too long and caused the deterioration of the rubber. If it is produced directly, it will also cause a burst. In this case, it is more difficult to analyze the quality.
Through the above introduction, China 20L Pail Mould Factory hopes that you can simply refer to the content of this article in future use.
https://www.rixiangmould.com/
There is also a kind of burst with just a light press. The position is mainly the bonding line, that is, when the injection point is designed by the injection molding manufacturer, the welding line is not designed in place, and the welding line is made on the top with the bump. It also depends on the thinner position outside. Especially in the production of ABS materials, it is easy to break. An experienced design engineer will first review the glue inlet point, and then drive the weld line to a position where it will not burst.
After the injection molding employees of the injection molding parts processing factory left their jobs for more than 20 minutes, when they returned to the job, they did not shoot out the waste rubber that had been in the barrel for too long and caused the deterioration of the rubber. If it is produced directly, it will also cause a burst. In this case, it is more difficult to analyze the quality.
Through the above introduction, China 20L Pail Mould Factory hopes that you can simply refer to the content of this article in future use.